What Thermoplastic Polyurethane (TPU) Is
Thermoplastic polyurethane, almost always abbreviated TPU, is a linear segmented polyurethane elastomer that softens on heating and can be melted, moulded and reprocessed repeatedly. That distinguishes it from cast, millable or crosslinked polyurethane systems, where covalent crosslinks lock the network in place and prevent remelting. TPU gets its strength from hard segments that associate into rigid domains; those associations are physical rather than chemical, so they loosen on heating and re-form on cooling. The result is a material that combines rubber-like elasticity with the processing economics of a thermoplastic: it can be injection moulded, extruded, calendered, blow-moulded into film, or dissolved in selected solvents for coatings and adhesives.
As a polymer, TPU does not have a single CAS Registry Number. Identity in the supply chain is established through the monomer set and the grade data sheet, and through the CAS numbers of the raw materials discussed below. Residual monomer content and the exact hard-segment content are the two figures that most often separate a general-purpose grade from a specialty grade at the same quoted hardness.
Polymer Architecture: Hard Segments, Soft Segments and Physical Crosslinking
TPU is a block copolymer assembled from three building blocks: a long-chain polyol that forms the soft segments, a diisocyanate, and a short-chain chain extender that together with the diisocyanate forms the hard segments. Because hard and soft blocks are chemically dissimilar, they separate into microphases. The hard phases act as physical crosslink points and load-bearing reinforcement, while the soft phases supply flexibility, damping and elastic recovery.
The hard segments associate through hydrogen bonding between urethane groups, producing rigid domains that hold the network together at service temperature. These domains are not permanent chemical crosslinks: they loosen when the material is heated and re-form as it cools, which is exactly why TPU is melt-processable and partly soluble in selected solvents, and why the material can be reground and remoulded within the limits set for the grade. The same physical network explains the difference in behaviour between grades of equal hardness: a higher hard-segment content raises modulus, tear strength and compression-set resistance, while a lower one improves softness and low-temperature flexibility.
Soft-segment chemistry sets the rest of the performance profile, in particular hydrolytic stability, low-temperature behaviour, oil resistance and light stability. Choosing the polyol is therefore the first decision in grade selection, and it matters more than the hardness number.
Raw Materials and Segment Chemistry
Diisocyanates. Aromatic MDI, diphenylmethane-4,4'-diisocyanate (CAS 101-68-8), is the workhorse of commodity TPU because it gives a good balance of strength, cost and processing latitude. Toluene diisocyanate, usually the 2,4-isomer (CAS 584-84-9) with the 2,6-isomer (CAS 91-08-7) as the co-isomer, is used in some high-performance and foam-related grades. Where colour stability and light resistance matter, aliphatic and cycloaliphatic diisocyanates are used instead: hexamethylene diisocyanate (CAS 822-06-0), isophorone diisocyanate (CAS 4098-71-9) and 4,4'-dicyclohexylmethane diisocyanate (CAS 5124-30-1). Aromatic grades yellow under ultraviolet exposure, which is why outdoor and transparent applications usually specify an aliphatic system or a well-stabilised compound.
Polyols for soft segments. Four families dominate. Polyester polyols, typically based on adipic acid reacted with a glycol, give high tensile strength, excellent abrasion resistance and good oil resistance but are the most sensitive to hydrolysis. Polyether polyols, based on propylene oxide or on polytetramethylene ether glycol produced from tetrahydrofuran (CAS 109-99-9), resist hydrolysis and microbial attack well and stay flexible at low temperature. Polycaprolactone polyols, made from caprolactone, sit between the two and are chosen for demanding long-life parts. Polycarbonate polyols give the best combination of hydrolytic and oxidative stability and are used in automotive, medical and outdoor applications where service life is measured in years. Polyether and polyester polyols are supplied as mixtures of oligomers and, as such, are described by their hydroxyl value and molecular weight rather than by a single CAS number; propylene oxide-based polyether polyols, for example, are commonly listed under CAS 25322-69-4.
Chain extenders. Short-chain diols form the hard segment with the diisocyanate. 1,4-Butanediol (CAS 110-63-4) is by far the most common, with 1,6-hexanediol (CAS 629-11-8) and ethylene glycol (CAS 107-21-1) used in specific systems, and aromatic diols such as hydroquinone bis(2-hydroxyethyl) ether (CAS 104-38-1) used where higher modulus and heat resistance are required. Diamine extenders produce urea linkages and a urethane-urea hard segment that hydrogen bonds more strongly.
Typical Property Profile and Test Methods
| Property | Typical range for commercial TPU | Common test method |
|---|---|---|
| Hardness | About Shore 70A to Shore 75D, grade dependent | Durometer hardness per ASTM D2240 and ISO 868; GB/T equivalents used domestically |
| Density | About 1.10 to 1.25 g/cm3 | Immersion density per ASTM D792 and ISO 1183 |
| Tensile strength | Roughly 20 to 55 MPa, higher for rigid grades | Tensile test per ASTM D412 and ISO 527; GB/T 1040 for plastics-type specimens |
| Elongation at break | Typically 300 to 700% | Same tensile test as above |
| Tear strength | Substantial, one of the material's advantages | ASTM D624 and ISO 34-1 |
| Compression set | Grade dependent; improved by higher hard-segment content | ASTM D395 and ISO 815 after 22 h at 70 C |
| Abrasion resistance | Very good; polyester grades generally best | DIN abrasion per ISO 4649 |
| Melt flow | Specified by grade at a defined temperature and load | Melt flow rate or melt volume rate per ASTM D1238 and ISO 1133; GB/T 3682 |
| Moisture content of pellets | Low; controlled before processing | Karl Fischer titration or loss-on-drying per the grade specification |
| Flex resistance at low temperature | Best for polyether and polycarbonate grades | Low-temperature impact and brittle-point tests |
The table shows the shape of the property envelope rather than a specification, because hardness and modulus are largely set by the hard-segment content while hydrolysis, oil and light resistance are set by the polyol. Two grades at Shore 85A can differ by a factor of two in flex fatigue life and by years in service life under humid conditions, depending on whether the soft segment is a polyester or a polycarbonate.
The Main TPU Types and How to Choose Between Them
By soft segment. Polyester TPU delivers the best combination of tensile strength, abrasion resistance and oil resistance at moderate cost, and is the usual choice for footwear, rollers, wheels and general technical parts in dry service. Polyether TPU resists hydrolysis and low-temperature stiffening, which makes it the default for cable and hose jacketing, outdoor parts and applications exposed to water or humidity. Polycaprolactone TPU offers good hydrolysis resistance combined with the mechanical profile of an ester grade. Polycarbonate TPU is the premium option where long-term hydrolytic and oxidative stability, weatherability and clarity are required.
By hard segment. Diol-extended systems give urethane hard segments; diamine-extended systems give urethane-urea hard segments with stronger hydrogen bonding, higher modulus and better heat resistance at the cost of a narrower processing window.
By crosslinking. Purely thermoplastic grades have a linear structure and can be remelted freely. So-called semi-thermoplastic grades contain a small amount of allophanate-type branching or crosslinking, which improves compression set and heat resistance but limits remelt and regrind use.
By product form. TPU is supplied as pellets for injection moulding and extrusion, as profile, tube, hose and rod, as film and sheet, and as solution grades in solvents such as dimethylformamide (CAS 68-12-2) or dimethylacetamide (CAS 127-19-5) for textile coatings, adhesives and laminating compounds. Solution grades must be handled with the engineering controls appropriate to the solvent carrier.
By hardness. Soft grades below Shore 80A behave as very flexible, skin-like materials for films and soft-touch parts. Mid-range grades between Shore 85A and Shore 95A cover most footwear, cable and general-purpose duties. Rigid grades from Shore 55D to 75D behave more like an engineering thermoplastic and are used for housings, gears, caster wheels and structural parts.
Processing: Moulding, Extrusion, Film and Solution Coatings
Injection moulding. TPU moulds on standard reciprocating-screw machines with general-purpose screws, and the main practical issues are drying, melt temperature control and adequate packing. Because the melt is shear sensitive, residence time and regrind ratio must stay inside the limits set for the grade; excessive regrind, or long hold-up at high temperature, degrades the polymer and produces surface defects, splay and loss of mechanical properties.
Extrusion. Tube, hose, profile, cable jacketing and wire coating are extruded from dried pellets using screws selected for elastomeric melts. Film is produced by blown-film or cast-film lines, and TPU film is also calendered. Extrusion grades are often supplied at a higher melt index than injection grades to keep melt pressure and die swell within the capability of the line.
Drying before processing. TPU absorbs atmospheric moisture, and residual water in the melt causes bubbles, silver streaking, surface defects and a measurable loss of tensile strength and elongation. Pellets are therefore dried in desiccant or dehumidifying dryers immediately before processing, and the residual moisture level is verified against the limit stated on the grade data sheet. This single step accounts for most processing complaints reported against the material.
Secondary operations. TPU can be welded by hot plate, ultrasonic and radio-frequency methods, printed, vacuum formed, laminated to textiles and foams, and solvent-bonded to itself and to rigid substrates. Adhesion to other polymers is generally achieved with a tie layer or a primer rather than by direct bonding.
Applications by Industry
Footwear. Soles, midsoles, outsoles, technical uppers, reinforcements, insoles and decorative components are the largest single TPU application. The material's combination of abrasion resistance, flex fatigue life and transparency makes it suitable both for functional midsoles and for translucent decorative details.
Cable, hose and wire. Abrasion-resistant jacketing, especially where cables must survive repeated flexing, dragging and contact with oils. Polyether grades dominate because they resist hydrolysis, and flame-retardant compounds are available where cable standards require it.
Film, sheet and laminates. Protective film, breathable membranes, laminating film for textiles, inflatable products such as airbags and bladders, and interlayers where toughness and transparency are required.
Industrial and mechanical. Conveyor belting, rollers, wheels, caster tyres, drive belts, seals, gaskets, bumpers, coupling elements, screen printing squeegees and mining screens where abrasion and impact are severe.
Automotive. Interior trim, seat components, gear knobs, cable sheathing, air ducts, weatherstrip components, protective film and under-hood parts in the heat-stabilised grades, plus clear protective film for paint protection.
Medical and personal care. Tubing, catheters, wound dressings, ostomy products, surgical drapes and wound-care film use aliphatic, low-colour grades that are often qualified to the biocompatibility standards applied to medical devices, including the ISO 10993 series and the United States Pharmacopeia plastic materials classification tests. Flexible, skin-friendly grades drive watch straps, mobile device protectors and textile coatings.
Adhesives and coatings. Solution and dispersion grades provide heat-activated adhesives, textile coatings, shoe adhesives and laminating systems that remain flexible at low temperature. Additive manufacturing. TPU filaments are used in fused deposition 3D printing for flexible, durable printed parts.
Quality Control, Moisture Control and Incoming Inspection
Because TPU properties depend on both chemistry and processing history, incoming inspection should combine a certificate of analysis review with a short set of confirmation tests. Hardness measured on a conditioned plaque, density, tensile strength and elongation at break, tear strength and compression set establish whether the lot matches the grade. Moisture content of the pellets must be measured before processing, since a lot that meets every mechanical specification can still fail on the line if it has absorbed water in transit or in storage.
Beyond the basic set, three checks repay the effort. Melt flow rate or melt volume rate at the grade's reference condition detects changes in molecular weight that will not be visible in the mechanical data of a compression-moulded plaque but will show up as inconsistent filling or sagging during extrusion. Colour and pellet geometry checks identify contamination and fines generation. And for outdoor, automotive or medical grades, hydrolysis resistance, heat ageing and ultraviolet exposure testing, or a review of the supplier's ageing data, should be carried out at qualification rather than left to service experience.
Batch traceability matters for another reason in this family: a change of polyol source, of chain extender ratio or of residual monomer level can shift performance without changing the hardness printed on the bag, so the grade designation alone is not a sufficient purchasing specification. Purchase against a written data-sheet specification with limits and test methods, and requalify whenever the specification changes.
Safety, Storage, Packaging and Regulatory Status
TPU pellets are not classified as a hazardous substance for transport or supply. The finished polymer contains only trace amounts of residual diisocyanate, and the handling risk in normal use is thermal rather than toxicological: molten polymer can cause burns, and overheating during processing can release decomposition products including diisocyanate vapour and carbon monoxide. Effective exhaust ventilation at the machine, adherence to the supplier's recommended processing window and avoidance of prolonged hold-up at excessive temperature are the essential engineering controls. Good practice also includes dust control when grinding, and local exhaust ventilation where grinding fines are generated.
Storage. Keep pellets in unopened moisture-barrier packaging in a dry, shaded warehouse at ambient temperature, away from direct sunlight, heat sources and strong odours, since TPU can pick up both moisture and odour from its surroundings. Sealed 25 kg bags, 500 to 1000 kg octabins and bulk containers with inner liners are common. Stacking heights should respect the bag specification to avoid block formation, and part-used bags should be resealed. Polyester grades are the most sensitive to moisture pick-up in storage; bags should be opened only when the material is to be used or dried.
Regulatory. Under REACH, polymers are exempt from registration while their monomers must be registered by the manufacturer or importer, so the compliance file for a TPU grade normally references the monomer registrations rather than the polymer itself. Food-contact grades are qualified against the applicable food-contact plastics rules, for example the polyurethane resin provisions in the United States food-additive regulations and the plastics regulation applicable in the European Union, plus the migration limits those rules set. Medical grades are supported by biocompatibility test data and by change-control agreements. Grades intended for electrical and electronic use should be checked against the substance restrictions applicable in the destination market, and safety data sheets for the polymer follow the ISO 11014 layout.
FAQ
Q: What is thermoplastic polyurethane TPU?
It is a linear segmented polyurethane elastomer built from a polyol, a diisocyanate and a chain extender. Hard segments associate into rigid physical crosslink domains while soft segments provide elasticity, so the material behaves like rubber in service but can be melted, moulded and reprocessed like a thermoplastic.
Q: How is TPU different from cast polyurethane?
Cast systems depend on chemical crosslinking and cannot be remelted. TPU contains little or no chemical crosslinking and derives its strength from reversible physical associations between hard segments, which is why TPU can be injection moulded, extruded and reground within grade limits.
Q: Which TPU type resists hydrolysis best?
Polyether-based grades resist hydrolysis far better than polyester-based grades, and polycarbonate-based grades are better still, which is why polyether and polycarbonate systems are specified for cable jacketing, humid service and long-life outdoor applications.
Q: Why must TPU pellets be dried before processing?
The polymer absorbs atmospheric moisture. Residual water in the melt turns to steam and causes bubbles, silver streaks and surface defects, and it also hydrolyses the polymer, reducing tensile strength and elongation. Pellets are therefore dried in a desiccant dryer immediately before processing and checked against the moisture limit on the data sheet.
Q: Does TPU have a CAS number?
TPU is a polymer and has no single CAS Registry Number; the monomers used to make it do, for example MDI CAS 101-68-8, 1,4-butanediol CAS 110-63-4 and hexamethylene diisocyanate CAS 822-06-0. Specification therefore relies on the supplier's grade data sheet, the monomer set and lot test data.
Q: Which hardness ranges are available?
Commercial TPU spans roughly Shore 70A to Shore 75D. Soft grades below Shore 80A suit films and soft-touch parts, the Shore 85A to 95A band covers most footwear, cable and general parts, and grades from Shore 55D to 75D behave like engineering thermoplastics for structural components.
Q: How should TPU be stored?
Keep sealed, moisture-barrier packaging in a dry, shaded warehouse away from heat, sunlight and strong odours, reseal part-used bags and use the material within the supplier's stated shelf life. Polyester grades are particularly sensitive to moisture picked up in storage, so bags should be opened only when the material is to be used or dried.